User profiles for M. Barash
Mark BarashAssociate Professor, Forensic Science Program Coordinator, Department of Justice Studies … Verified email at sjsu.edu Cited by 1078 |
[HTML][HTML] Forensic autosomal short tandem repeats and their potential association with phenotype
Forensic DNA profiling utilizes autosomal short tandem repeat (STR) markers to establish
identity of missing persons, confirm familial relations, and link persons of interest to crime …
identity of missing persons, confirm familial relations, and link persons of interest to crime …
The UDP-N-acetylglucosamine 2-epimerase/N-acetylmannosamine kinase gene is mutated in recessive hereditary inclusion body myopathy
… b, Sequence chromatograms from a healthy (WT) and a diseased (M) genotype for the …
Nazarian for her extensive efforts and our special thanks to M. Banayan for his endless and …
Nazarian for her extensive efforts and our special thanks to M. Banayan for his endless and …
Complexity in manufacturing systems, Part 1: Analysis of static complexity
AV Deshmukh, JJ Talavage, MM Barash - IIE transactions, 1998 - Taylor & Francis
This paper studies static complexity in manufacturing systems. We enumerate factors
influencing static complexity, and define a static complexity measure in terms of the processing …
influencing static complexity, and define a static complexity measure in terms of the processing …
Public-sector design/build evolution and performance
KR Molenaar, AD Songer, M Barash - Journal of management in …, 1999 - ascelibrary.org
Design/build project delivery is experiencing expansive growth in both the private and the
public sectors. Owners are driving the change away from the traditional design/bid/build …
public sectors. Owners are driving the change away from the traditional design/bid/build …
A mathematical approach to automatic configuration of machining fixtures: analysis and synthesis
Drawing on screw theory and engineering mechanics, a mathematical theory for automatic
configuration of machining fixtures for prismatic parts is developed. There are two parts in the …
configuration of machining fixtures for prismatic parts is developed. There are two parts in the …
Experimental investigation on CBN turning of hardened AISI 52100 steel
YK Chou, CJ Evans, MM Barash - Journal of Materials Processing …, 2002 - Elsevier
This study investigated the performance and wear behavior of different cubic boron nitride (CBN)
tools in finish turning of hardened AISI 52100 steel. Tool performance was evaluated …
tools in finish turning of hardened AISI 52100 steel. Tool performance was evaluated …
Effect of hardness on the surface integrity of AISI 4340 steel
Y Matsumoto, MM Barash, CR Liu - 1986 - asmedigitalcollection.asme.org
… Liu and Barash [12] found that the shear plane instead of ploughing force or anything else, …
the grain size is very small, probably 0.05 to 0.5 m. There were some oxides (Fe304) on the …
the grain size is very small, probably 0.05 to 0.5 m. There were some oxides (Fe304) on the …
Variables governing patterns of mechanical residual stress in a machined surface
CR Liu, MM Barash - 1982 - asmedigitalcollection.asme.org
… flank wear with negative clearance angles in this study), there will be a stretching force on
the line element m' n' due to friction. This means that the line element mn is further subjected …
the line element m' n' due to friction. This means that the line element mn is further subjected …
[HTML][HTML] Lidocaine-induced methemoglobinemia: a clinical reminder
M Barash, KA Reich, D Rademaker - Journal of Osteopathic Medicine, 2015 - degruyter.com
… The hereditary form is associated with a deficiency of intrinsic cytochrome b5-MetHb
reductase or with the presence of congenital hemoglobin M, a form of hemoglobin unable to bind …
reductase or with the presence of congenital hemoglobin M, a form of hemoglobin unable to bind …
The mechanical state of the sublayer of a surface generated by chip-removal process—Part 1: Cutting with a sharp tool
CR Liu, MM Barash - 1976 - asmedigitalcollection.asme.org
… A specimen was cut with a tool with 0.254 mm (0.010 in.) flank wear at the highest cutting
speed 277.37 m/min (910 sfm) used in this investigation. The depth of cut was 0.254 mm (…